Polymer Property : Tensile Strength = 1010 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength 6.96 MPa
1010 psi
Silicone Property; ASTM D412
Arlon 56344R025 0.025" (0.635 mm) Semi-cured Silicone Rubber
Design/Construction: Interleave: PolyethyleneSide 1: Semi-Cured Silicone Rubber Substrate: 1564 Style FiberglassAppearance: Red silicone gum on fiberglass clothThis data represents typical values fo..
Tensile Strength 6.96 MPa
1010 psi
Silicone Property; ASTM D412
Arlon 51344R025 0.025" (0.635 mm) Semi-Cured Silicone Rubber with Fiberglass Substrate
Design/Construction: Interleave: Polyethylene Side 1: Semi-Cured Silicone RubberSubstrate: Style 7628 FiberglassAppearance: Red silicone gum on fiberglass clothThis data represents typical values fo..