Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength | 6.96 MPa | 1010 psi | Silicone Property; ASTM D412 |
Arlon 56344R025 0.025" (0.635 mm) Semi-cured Silicone Rubber Design/Construction: Interleave: PolyethyleneSide 1: Semi-Cured Silicone Rubber Substrate: 1564 Style FiberglassAppearance: Red silicone gum on fiberglass clothThis data represents typical values fo.. |
|||
Tensile Strength | 6.96 MPa | 1010 psi | Silicone Property; ASTM D412 |
Arlon 51344R025 0.025" (0.635 mm) Semi-Cured Silicone Rubber with Fiberglass Substrate Design/Construction: Interleave: Polyethylene Side 1: Semi-Cured Silicone RubberSubstrate: Style 7628 FiberglassAppearance: Red silicone gum on fiberglass clothThis data represents typical values fo.. |