Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength | >= 11.3 MPa | >= 1640 psi | ASTM D 638 |
Karina 700D48/1-IS Black PVC Compound PVC Compound recommended for automotive parts injection. Also recommended for retractable telephone wire sheeting.Information provided by Karina Indústria e Comércio de Plásticos Ltda. |