Polymer Property : Tensile Strength = 1640 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength >= 11.3 MPa
>= 1640 psi
ASTM D 638
Karina 700D48/1-IS Black PVC Compound
PVC Compound recommended for automotive parts injection. Also recommended for retractable telephone wire sheeting.Information provided by Karina Indústria e Comércio de Plásticos Ltda.