Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength | 13.4 MPa | 1940 psi | ASTM D412 |
S&E Specialty Polymers TufTech™ GM-3236 PVC Compound Application: A non-toxic PVC based compound designed for general purpose profile extrusion applications.Information provided by S&E Specialty Polymers |
|||
Tensile Strength | 13.4 MPa | 1950 psi | |
AlphaGary Garaflex™ E X 00-207F UV-FG LCF Vinyl Thermoplastic Elastomer Garaflex™ E is a vinyl based thermoplastic elastomer used mostly in wire and cable105°C rated flame retardant, flexible jacket compound with sunlight & fungus resistant properties |
|||
Tensile Strength | 13.4 MPa | 1940 psi | ISO 37 |
AlphaGary Evoprene™ G 975 SEBS Thermoplastic Elastomer Evoprene™ G compounds are styrene – ethylene butylene –styrene base thermoplastic elastomer with related hydrogenated block copolymers. These polymers are fully saturated so the resistance to oxi.. |