Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength | 7.45 - 9.10 MPa | 1080 - 1320 psi | Compound Property |
Arlon 10502N060 0.060" (1.52 mm) Cured/Post-Cured Unsupported Silicone Rubber Design/Construction:Side 1: Cured/Post-Cured Unsupported Silicone Rubber Appearance: Red silicone rubberThis data represents typical values for the production material. The data should not be used t.. |
|||
Tensile Strength | 7.45 - 9.10 MPa | 1080 - 1320 psi | Compound Property |
Arlon 10502R010 0.010" (.254 mm) Cured/Post-Cured Unsupported Silicone Rubber Design/Construction:Side 1: Cured/Post-Cured Unsupported Silicone RubberAppearance: Red silicone rubberThis data represents typical values for the production material. The data should not be used to.. |
|||
Tensile Strength | 7.45 - 9.10 MPa | 1080 - 1320 psi | Compound Property |
Arlon 10502R030 0.040" (1.02 mm) Cured/Post-Cured Unsupported Silicone Rubber Design/Construction:Side 1: Cured/Post-Cured Unsupported Silicone Rubber Appearance: Red silicone rubberThis data represents typical values for the production material. The data should not be used t.. |
|||
Tensile Strength | 7.45 - 9.10 MPa | 1080 - 1320 psi | |
Arlon 10502R125 Cured/Post-cured, Unsupported Silicone Rubber Product Color: RedInterleave: 0.003" PolyethyleneThis data represents typical values for the production material and should not be used as material specifications.Information provided by ARLON Silic.. |