Mechanical Properties Metric English Comments
Tensile Strength 145 MPa
21000 psi
ASTM D-638
PlastiComp Complet® LGF30-PBT Polybutylene Terephthalate, 30% Long Glass Fiber Reinforced
Complēt® long-fiber reinforced pellets are manufactured to exceed expectation for quality and performance.Polybutylene Terephthalate (PBT) with 30% long glass fiber reinforcementInformation pr..
Tensile Strength 145 MPa
21000 psi
ASTM D-638
PlastiComp Complet® LCF10/LGF30 - PP Polypropylene, 40% Long Carbon/Glass Fiber
Composite PelletsInformation provided by PlastiComp, Inc.
Tensile Strength 145 MPa
21000 psi
ASTM D-638
PlastiComp Complet® LGF20 - TPU Rigid Thermoplastic Polyurethane, 20% Long Glass Fiber Reinforced
Complet® long-fiber reinforced pellets are manufactured to exceed expectation for quality and performance.Polyurethane with 20% long glass fiber reinforcementInformation provided by PlastiComp, Inc..
Tensile Strength 145 MPa
21000 psi
ASTM D-638
PlastiComp Complet® LGF40-PA12 Nylon 12, 40% Long Glass Fiber Reinforced
Complēt® long-fiber reinforced pellets are manufactured to exceed expectation for quality and performance.Nylon 12 with 40% long glass fiber reinforcementInformation provided by PlastiComp, In..
Tensile Strength 145 MPa
21000 psi
ASTM D638
Solvay Specialty Polymers Ryton® BR111BL Polyphenylene Sulfide (PPS), GlassMineral Filled
Ryton® BR111BL Ryton® BR111 is a black-colored glass fiber and mineral filled polyphenylene sulfide compound that provides enhanced mechanical strength with good electrical properties and outs..
Tensile Strength 145 MPa
21000 psi
ASTM D638
Techmer ES Luriblend® PA6/6 CF10 TL15 BK 10% Carbon Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Carbon Fiber, 10% Filler by WeightAdditive: PTFE + Silicone Lubricant(15%)Features: Lubricated and Good Wear ResistanceAppearance: Blac..
Tensile Strength 145 MPa
21000 psi
ASTM D638
Teknor Apex Chemlon® 233 GI Nylon 6, 33% Glass Fiber Reinforced
Features: High Impact, 33% Glass Reinforced; Highly toughened compound exhibiting strength and rigidity; Good Creep Resistance; Good Stiffness; Good Toughness; Impact Modified Processing Method: Inj..
Tensile Strength 145 MPa
21000 psi
ASTM D638
Teknor Apex Chemlon® 233 GVH Nylon 6, 33% Glass Fiber Reinforced
Features: Flame Retardant; Good Stiffness; High Strength Processing Method: Injection Method Forms: Pellets Additive: Flame RetardantInformation Provided by Teknor Apex