Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Teknor Apex Chemlon® 233 GI Nylon 6, 33% Glass Fiber Reinforced

Category Polymer , Thermoplastic , Nylon , Nylon 6 , Nylon 6, 30% Glass Fiber Filled
Manufacturer Teknor Apex Company
Trade Name Chemlon®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Teknor Apex Chemlon® 233 GI Nylon 6, 33% Glass Fiber Reinforced.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Features: High Impact, 33% Glass Reinforced; Highly toughened compound exhibiting strength and rigidity; Good Creep Resistance; Good Stiffness; Good Toughness; Impact Modified Processing Method: Injection MoldingForms: Pellets Additive: Impact ModifierInformation Provided by Teknor Apex
Physical Properties Metric English Comments
Specific Gravity 1.35 g/cc
1.35 g/cc
ASTM D792
Mechanical Properties Metric English Comments
Tensile Strength 145 MPa
21000 psi
ASTM D638
Elongation at Break 3.0 %
3.0 %
ASTM D638
Flexural Strength 203 MPa
29500 psi
ASTM D790
Flexural Modulus 6.89 GPa
1000 ksi
ASTM D790
Izod Impact, Notched 1.87 J/cm

@Temperature 22.8 °C
3.50 ft-lb/in

@Temperature 73.0 °F
ASTM D256
Processing Properties Metric English Comments
Melt Temperature 216 °C
420 °F
Descriptive Properties Value Comments
Appearance Black; Natural Color