Mechanical Properties Metric English Comments
Tensile Strength 10.89 MPa

@Temperature 121 °C,
Time 605000 sec
1579 psi

@Temperature 250 °F,
Time 168 hour
Aged
S&E Specialty Polymers TufGuard E™ CPE 12-020 CPE, Flame Retardant
Application: A 90°C, oil resistant; CPE based FT4, (210,000 BTU) Wire & Cable jacketing compound with enhanced low temperature properties.Information provided by S&E Specialty Polymers