Material Notes:
Application: A 90°C, oil resistant; CPE based FT4, (210,000 BTU) Wire & Cable jacketing compound with enhanced low temperature properties.Information provided by S&E Specialty Polymers
Physical Properties Metric English Comments
Specific Gravity 1.37 g/cc
1.37 g/cc
ASTM D792
Mechanical Properties Metric English Comments
Hardness, Shore A 85.0

@Time 15.0 sec
85.0

@Time 0.00417 hour
ASTM D2240
Tensile Strength 12.1 MPa
1750 psi
ASTM D412
8.47 MPa

@Temperature 100 °C,
Time 346000 sec
1230 psi

@Temperature 212 °F,
Time 96.0 hour
Oil Aged
10.89 MPa

@Temperature 121 °C,
Time 605000 sec
1579 psi

@Temperature 250 °F,
Time 168 hour
Aged
Elongation at Break 350 %
350 %
ASTM D412
231 %

@Treatment Temp. 100 °C,
Time 346000 sec
231 %

@Treatment Temp. 212 °F,
Time 96.0 hour
Oil Aged
315 %

@Treatment Temp. 121 °C,
Time 605000 sec
315 %

@Treatment Temp. 250 °F,
Time 168 hour
Aged
Thermal Properties Metric English Comments
Brittleness Temperature -33.0 °C
-27.4 °F
ASTM D746
Oxygen Index >= 37.0 %
>= 37.0 %
ASTM D2863