Polymer Property : Tensile Strength = 17100 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength 118 MPa
17100 psi
ASTM D638
Kolon KOPA® KN333G15SIBL G/F Reinforced Nylon 66
High strength, high toughnessApplications Relay coversInformation provided by API-Kolon.
Tensile Strength 118 MPa
17100 psi
ASTM D638
Gromax PBT 4130-104D 30% Glass Fiber Filled
Product Description: A glass fiber 30% reinforced injection molding grade. Characteristics:Excellent electrical property Excellent temperature resistance, high heat distortion temperature Excellent ..
Tensile Strength 118 MPa
17100 psi
ASTM D638
Gromax PBT 3030-104 30% Glass Fiber Filled
Product Description: A glass fiber 30% reinforced injection molding grade. Characteristics:Excellent electrical property Excellent temperature resistance, high heat distortion temperature Excellent ..
Tensile Strength 118 MPa
17100 psi
ASTM D638
Samyang Tribit® 1551GN30 PBT, Impact
Crystallization is fast, formability is excellent and thermal resistance, chemical resistance, electrical properties and abrasion resistance are excellent.1551GN30 is an impact grade.Information pro..
Tensile Strength 118 MPa
17100 psi
5 mm/min; ISO 527-1
Sax Polymers SAXAMID 226F4RY01 Nylon 6.6, 20% Glass Fiber
SAXAMID 226F4RY01 is a polyamide 6.6 injection-molding-grade reinforced with 20% glass fibers. It has a halogen-free flame retardant.Information provided by SAX Polymers
Tensile Strength 118 MPa
17100 psi
ASTM D638
Ensinger Tecapeek® XP-112 Compression Molded PEEK Compound, 20% Carbon Fiber
Ensinger Special Polymers offers over twenty different VICTREX® PEEK blends to choose from and has the capability to blend custom compounds for specific applications. Compression molding results in..
Tensile Strength 118 MPa

@Temperature 120 °C
17100 psi

@Temperature 248 °F
BASF Ultramid® Structure B3WG10 LF High-Performance Long-Glass Fiber Reinforced Polyamide
Tensile Strength 118 MPa
17100 psi
ASTM D638
Gromax CCP PBT 4830-BK 30% Glass Fiber Filled
Product Description: A glass fiber 30% reinforced injection molding grade. Characteristics:Excellent electrical property Excellent temperature resistance, high heat distortion temperature Excellent ..