Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength | 100 - 120 MPa | 14500 - 17400 psi | Injection and Compression; ISO 527 |
Raschig Group EPOXIDUR® 3585 EP Epoxy, Molded, Glass Fiber Filler Glass-fiber reinforced and inorganically filled epoxy molding compound. Good mechanical strength, very good electrical isolation properties and dimensional stability even at high temperatures, excel.. |
|||
Tensile Strength | 100 - 120 MPa | 14500 - 17400 psi | Injection; ISO 527 |
Raschig Group RESINOL® 400 EPF Phenolic Glass-fiber reinforced phenolic molding compound. Excellent heat resistance, low mould shrinkage and post-shrinkage, good chemical resistance and very good mechanical properties. This product meets .. |