Mechanical Properties Metric English Comments
Tensile Strength 13.0 - 18.0 MPa
1890 - 2610 psi
ASTM D4894
Isoflon PTFE + 25% Carbon Polytetrafluoroethylene with 25% Carbon
Properties:Improved compression and wear resistanceGood thermal conductivityLow permeabilityImproved coefficient of thermal expansion when combined with ceramicApplications: Seals recommended for h..
Tensile Strength 13.0 - 18.0 MPa
1890 - 2610 psi
ASTM D4894
Isoflon PTFE + 25% Glass Polytetrafluoroethylene with 25% Glass
Properties:Improved compression and wear resistanceExcellent chemical stabilityBetter thermal conductivityApplications: Dynamic seals with rotating or alternating motion.Information provided by Iso..
Tensile Strength 14.0 - 18.0 MPa
2030 - 2610 psi
molded; ASTM D4894, ASTM D4745
Guarniflon PTFE G453 Polytetrafluoroethylene 25% Carbographite
PTFE G Standard Compound with carbon..Properties: Good thermal and electrical conductivity. Good resistance to deformation. Excellent resistance to load with low coefficient of friction and high ..
Tensile Strength 13.0 - 18.0 MPa
1890 - 2610 psi
ASTM D4894
Isoflon PTFE +28% GL Blue-E glass-1% Blue Polytetrafluoroethylene with 28% GL-Blue-E glass-1% Blue (equivalent VX1)
Properties:Improved compression and wear resistanceExcellent chemical stabilityBetter thermal conductivityInformation provided by Isoflon.