Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength | 23.0 MPa | 3340 psi | ISO 527 |
Murtfeldt Original Material ”S”® plus + TLS Polyethylene Original Material ”S”® plus+ TLS is designed for high temperature industrial applications for which Original Material ”S”® could previously not be used. The thermal oxidation point has been i.. |
|||
Tensile Strength | 23.0 MPa | 3340 psi | at Yield; ISO 527-1/-2 |
Quadrant EPP Borotron® HM PE-HMW + boron based additive (ISO Data) Borotron UH and Borotron HM are boron loaded PE-(U)HMW grades, specifically developed for neutron shielding purposes in nuclear installations. The high hydrogen content of PE-(U)HMW makes it very su.. |
|||
Tensile Strength | 23.0 MPa | 3340 psi | |
Imerys ImerPlastâ„¢ 20 Recycled Polyolefin for Pipe Extrusion High Stiffness Polyolefin/Mineral CompoundInformation provided by Imerys. |
|||
Tensile Strength | 23.0 - 28.0 MPa | 3340 - 4060 psi | molded; ASTM D4745 |
Guarniflon PTFE G416 Polytetrafluoroethylene 40% Bronze, 2% Carbon PTFE G Special Compound with bronze Properties: Enhanced compressive strength. Good wear resistance and high thermal conductivity.Application: Unlubricated bearings for high speed excluding hard .. |
|||
Tensile Strength | 23.0 - 28.0 MPa | 3340 - 4060 psi | molded; ASTM D4745 |
Guarniflon PTFE G427 Polytetrafluoroethylene 40% Bronze, 5% Molybdenum Disulfide PTFE G Special Compound with bronze and molybdenum disulphiteInformation provided by Guarniflon® |
|||
Tensile Strength | 23.0 - 28.0 MPa | 3340 - 4060 psi | molded; ASTM D4745 |
Guarniflon PTFE G436 Polytetrafluoroethylene 3% Molybdenum Disulfide PTFE G Standard Compound with molybdenum disulphite. Enhanced non-stick properties. Low static coefficient of friction. Fairly good resistance to deformation. Applications: Guide bands. Details ne.. |
|||
Tensile Strength | 23.0 MPa | 3340 psi | ASTM D412 |
Wanhua Chemical Wanthane® WHT-8280 Polyether-Based TPU Excellent transparency, short cycle time, hydrolytic stability, fungus resistance, low temperature flexibility, UV resistanceInformation provided by Wanhua Chemical Group Co., Ltd. |
|||
Tensile Strength | 23.0 MPa @Strain 100 % |
3340 psi @Strain 100 % |
ISO 37 |
BASF Elastollan S 64 D TPUR Description: Thermoplastic Polyester Polyurethane Elastomers with excellent mechanical properties and wear resistance, good damping characteristics and a high resilience performance.Typical Applicat.. |
|||
Tensile Strength | 23.0 MPa @Strain 300 % |
3340 psi @Strain 300 % |
ISO 37 |
BASF Elastollan S 98 A TPUR Description: Thermoplastic Polyester Polyurethane Elastomers with excellent mechanical properties and wear resistance, good damping characteristics and a high resilience performance.Typical Applicat.. |
|||
Tensile Strength | >= 23.0 MPa | >= 3340 psi | ISO 37 |
Austin Novel Materials Texalan® 370A Polyester-based TPU Description: Good abrasion resistance, tensile strength, oil resistance which can be used in injection, extrusion purpose.Information from Dawnentech |