Polymer Property : Tensile Strength = 3340 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength 23.0 MPa
3340 psi
ISO 527
Murtfeldt Original Material ”S”® plus + TLS Polyethylene
Original Material ”S”® plus+ TLS is designed for high temperature industrial applications for which Original Material ”S”® could previously not be used. The thermal oxidation point has been i..
Tensile Strength 23.0 MPa
3340 psi
at Yield; ISO 527-1/-2
Quadrant EPP Borotron® HM PE-HMW + boron based additive (ISO Data)
Borotron UH and Borotron HM are boron loaded PE-(U)HMW grades, specifically developed for neutron shielding purposes in nuclear installations. The high hydrogen content of PE-(U)HMW makes it very su..
Tensile Strength 23.0 MPa
3340 psi
Imerys ImerPlastâ„¢ 20 Recycled Polyolefin for Pipe Extrusion
High Stiffness Polyolefin/Mineral CompoundInformation provided by Imerys.
Tensile Strength 23.0 - 28.0 MPa
3340 - 4060 psi
molded; ASTM D4745
Guarniflon PTFE G416 Polytetrafluoroethylene 40% Bronze, 2% Carbon
PTFE G Special Compound with bronze Properties: Enhanced compressive strength. Good wear resistance and high thermal conductivity.Application: Unlubricated bearings for high speed excluding hard ..
Tensile Strength 23.0 - 28.0 MPa
3340 - 4060 psi
molded; ASTM D4745
Guarniflon PTFE G427 Polytetrafluoroethylene 40% Bronze, 5% Molybdenum Disulfide
PTFE G Special Compound with bronze and molybdenum disulphiteInformation provided by Guarniflon®
Tensile Strength 23.0 - 28.0 MPa
3340 - 4060 psi
molded; ASTM D4745
Guarniflon PTFE G436 Polytetrafluoroethylene 3% Molybdenum Disulfide
PTFE G Standard Compound with molybdenum disulphite. Enhanced non-stick properties. Low static coefficient of friction. Fairly good resistance to deformation. Applications: Guide bands. Details ne..
Tensile Strength 23.0 MPa
3340 psi
ASTM D412
Wanhua Chemical Wanthane® WHT-8280 Polyether-Based TPU
Excellent transparency, short cycle time, hydrolytic stability, fungus resistance, low temperature flexibility, UV resistanceInformation provided by Wanhua Chemical Group Co., Ltd.
Tensile Strength 23.0 MPa

@Strain 100 %
3340 psi

@Strain 100 %
ISO 37
BASF Elastollan S 64 D TPUR
Description: Thermoplastic Polyester Polyurethane Elastomers with excellent mechanical properties and wear resistance, good damping characteristics and a high resilience performance.Typical Applicat..
Tensile Strength 23.0 MPa

@Strain 300 %
3340 psi

@Strain 300 %
ISO 37
BASF Elastollan S 98 A TPUR
Description: Thermoplastic Polyester Polyurethane Elastomers with excellent mechanical properties and wear resistance, good damping characteristics and a high resilience performance.Typical Applicat..
Tensile Strength >= 23.0 MPa
>= 3340 psi
ISO 37
Austin Novel Materials Texalan® 370A Polyester-based TPU
Description: Good abrasion resistance, tensile strength, oil resistance which can be used in injection, extrusion purpose.Information from Dawnentech