Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength | 1590 MPa | 230000 psi | 48 HRC |
Schmolz + Bickenbach Thermodur® 2344 Magnum Hot Work Die Steel Description: Thermodur® 2344 Magnum is an electro slag remelted (ESR) hot work die steel, designed to meet all die casting industry specificationCharacteristics: Excellent toughness; Excellent re.. |
|||
Tensile Strength | 1590 MPa | 230000 psi | 44-48 HRC |
Schmolz + Bickenbach Thermodur® 2714 Extra Fine Structure - Hot Work Die Steel Description: Thermodur 2714 is an Extra Fine Structure (EFS) nickel based tool steel.Characteristics: Excellent high temperature strength; Good toughness; and Good resistance to thermal shockApplica.. |
|||
Tensile Strength | 1590 MPa | 230000 psi | |
Wingate Alloys Winco-Tuf 40IT Ultra High Strength, Thru-Hardened Alloy Wear Plate For extreme abrasion and moderate impact.Winco-Tuf 40 has excellent toughness at high hardness and in heavy sections. For severe impact and abrasions.Advantages: Maximum resistance to abrasion and i.. |