Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Wingate Alloys Winco-Tuf 40IT Ultra High Strength, Thru-Hardened Alloy Wear Plate

Category Metal , Ferrous Metal , Alloy Steel
Manufacturer Wingate Alloys
Trade Name Winco-Tuf
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Wingate Alloys Winco-Tuf 40IT Ultra High Strength, Thru-Hardened Alloy Wear Plate.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
For extreme abrasion and moderate impact.Winco-Tuf 40 has excellent toughness at high hardness and in heavy sections. For severe impact and abrasions.Advantages: Maximum resistance to abrasion and impact.Added nickel provides improved toughness and improved corrosion-resistance.Withstands the brittleness which develops at subnormal temperatures.Increased toughness and fatigue resistance.Retains high strength and wearability at high temperatures.High impact and wear properties retained at weld joints.Information from Wingate Alloys Inc.
Mechanical Properties Metric English Comments
Hardness, Brinell 420 - 455
420 - 455
Hardness, Rockwell C 40 - 48
40 - 48
Tensile Strength 1590 MPa
230000 psi
Tensile Strength, Yield 1320 MPa
191500 psi
Elongation at Break 17.4 %
17.4 %
2[in]
Reduction of Area 55 %
55 %
Charpy Impact 40.7 J
30.0 ft-lb
Component Elements Properties Metric English Comments
Carbon, C 0.20 - 0.28 %
0.20 - 0.28 %
Chromium, Cr 1.1 - 1.75 %
1.1 - 1.75 %
Copper, Cu 0.15 - 0.30 %
0.15 - 0.30 %
Iron, Fe 95.27 - 97 %
95.27 - 97 %
Manganese, Mn 0.80 - 1.0 %
0.80 - 1.0 %
Molybdenum, Mo 0.15 - 0.35 %
0.15 - 0.35 %
Nickel, Ni 0.40 - 0.70 %
0.40 - 0.70 %
Phosphorous, P <= 0.025 %
<= 0.025 %
Silicon, Si 0.20 - 0.30 %
0.20 - 0.30 %
Sulfur, S <= 0.025 %
<= 0.025 %
Users viewing this material also viewed the following: