Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength | 20.13 MPa @Treatment Temp. 136 °C, Time 605000 sec |
2920 psi @Treatment Temp. 277 °F, Time 168 hour |
Air Oven aged |
S&E Specialty Polymers GA-1042LF PVC Application: UL bulletinized PVC based compound, suitable for injection molding application.Information provided by S&E Specialty Polymers |