Polymer Property : Tensile Strength = 30.36 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength 30.36 MPa
4404 psi
ASTM D638
Shuman SP810 Black Polystyrene High Impact
Good impact strength, easy processability, good surface appearance, ULInformation provided by Shuman Plastics, Inc.
Tensile Strength 30.36 MPa
4404 psi
ASTM D638
Shuman SP880 Grey Polystyrene High Impact
Good impact strength, easy processability, good surface appearance, ULInformation provided by Shuman Plastics, Inc.