Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength | 30.36 MPa | 4404 psi | ASTM D638 |
Shuman SP810 Black Polystyrene High Impact Good impact strength, easy processability, good surface appearance, ULInformation provided by Shuman Plastics, Inc. |
|||
Tensile Strength | 30.36 MPa | 4404 psi | ASTM D638 |