Polymer Property : Tensile Strength = 32300 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength 223 MPa
32300 psi
ASTM D638
Solvay Specialty Polymers KetaSpire® KT-880 CF30 Polyetheretherketone (PEEK)  (Unverified Data**)
KetaSpire KT-880 CF30 is a high flow, 30% carbon fiber reinforced grade of polyetheretherketone (PEEK). Carbon-fiber reinforcement of KetaSpire PEEK provides the maximum levels of mechanical propert..
Tensile Strength 223 MPa
32300 psi
ASTM D638
Solvay Specialty Polymers KetaSpire® KT-880 CF30 Polyetheretherketone (PEEK), 30% Carbon Fiber
KetaSpire® KT-880 CF30 is a high flow, 30% carbon fiber reinforced grade of polyetheretherketone (PEEK). Carbon-fiber reinforcement of KetaSpire® PEEK provides the maximum levels of mechanical..