Mechanical Properties Metric English Comments
Tensile Strength 27.6 - 34.5 MPa
4000 - 5000 psi
ASTM D638
Mar-Bal MB2000-5 Thermoset Polyester Composite Molding Compound
An excellent flame and track resistant material with excellent electrical and mechanical properties. Good dielectric strength and low shrink for close dimensional control.Mar-Bal standard grades can..
Tensile Strength 27.6 - 34.5 MPa
4000 - 5000 psi
ASTM D638
Mar-Bal MB2000-8 Thermoset Polyester Composite Molding Compound
An excellent flame and track resistant material with excellent electrical and mechanical properties. Good dielectric strength and low shrink for close dimensional control.Mar-Bal standard grades can..