Mechanical Properties Metric English Comments
Tensile Strength 2.40 MPa

@Strain 100 %
348 psi

@Strain 100 %
ISO 37
BASF Elastollan S 60 A SPF TPUR
Description: Thermoplastic Polyester Polyurethane Elastomers with excellent mechanical properties and wear resistance, good damping characteristics and a high resilience performance.Typical Applicat..
Tensile Strength 2.40 MPa
348 psi
average; in the plane; ISO 527 1-2
3A Composites Core Materials AIREX® R63.140 Damage Tolerant Foam
AIREX® R63 is a closed-cell, linear, thermoplastic polymer foam with extremely high damage tolerance. This formula combines high elongation and excellent bond strength. AIREX® R63 is cold formable..
Tensile Strength 2.40 MPa
348 psi
Measured on compression molded slabs; ISO 37
Kraton® D1119 B (SIS) Linear Triblock Copolymer
Description: Kraton D1119 B is a clear, linear triblock copolymer based on styrene and isoprene with a polystyrene content of 22%. It is supplied from South America in the physical form identified: ..
Tensile Strength 2.40 MPa
348 psi
Typical properties on film cast from toluene solution; ASTM D412
Kraton® D1119 P (SIS) Linear Triblock Copolymer
Description: Kraton D1119 P is a clear, linear triblock copolymer based on styrene and isoprene with a polystyrene content of 22%. It is supplied from North America in the physical form identified: ..
Tensile Strength 2.40 MPa
348 psi
ISO 37
AlphaGary Evoprene™ GC 5694 SEBS Thermoplastic Elastomer
Evoprene™ GC compounds are based on styrene ethylene- butylene styrene block copolymers. Evoprene™ GC series was created to provide cost effective solutions for processors and end users alike. Can..