Polymer Property : Tensile Strength = 4122 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength 28.42 MPa

@Temperature 75.0 °C,
Time 4.838e+6 sec
4122 psi

@Temperature 167 °F,
Time 1344 hour
Immersion in Water
Lubrizol ESTANE® 58300 Ether Based Thermoplastic Polyurethane
Features: Good physical properties, hydrolysis resistance, low temperature performance and abrasion with a wide processing window for extrusion.Uses: Blown and flat die/cast film extrusion, Injectio..