Category Polymer , Thermoplastic , Elastomer, TPE , Polyurethane, TP , Thermoplastic Polyurethane, Elastomer, Ether Grade
Manufacturer Lubrizol (former Noveon)
Trade Name ESTANE®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Lubrizol ESTANE® 58300 Ether Based Thermoplastic Polyurethane.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Features: Good physical properties, hydrolysis resistance, low temperature performance and abrasion with a wide processing window for extrusion.Uses: Blown and flat die/cast film extrusion, Injection molding and cable jacketing.Information provided by Lubrizol
Physical Properties Metric English Comments
Specific Gravity 1.10 g/cc
1.10 g/cc
ASTM D792
Maximum Moisture Content 0.020
0.020
Mechanical Properties Metric English Comments
Hardness, Shore A 82

@Time 5.00 sec
82

@Time 0.00139 hour
ASTM D2240
Tensile Strength 37.9 MPa
5500 psi
ASTM D412
28.42 MPa

@Temperature 75.0 °C,
Time 4.838e+6 sec
4122 psi

@Temperature 167 °F,
Time 1344 hour
Immersion in Water
29.18 MPa

@Temperature 75.0 °C,
Time 2.59e+6 sec
4232 psi

@Temperature 167 °F,
Time 720 hour
Immersion in Water
29.94 MPa

@Temperature 75.0 °C,
Time 1.21e+6 sec
4342 psi

@Temperature 167 °F,
Time 336 hour
Immersion in Water
30.69 MPa

@Temperature 75.0 °C,
Time 605000 sec
4451 psi

@Temperature 167 °F,
Time 168 hour
Immersion in Water
37.9 MPa

@Temperature 75.0 °C,
Time 0.000 sec
5500 psi

@Temperature 167 °F,
Time 0.000 hour
Immersion in Water
Elongation at Break 700 %
700 %
ASTM D412
100% Modulus 0.00480 GPa
0.696 ksi
ASTM D412
300% Modulus 0.00760 GPa
1.10 ksi
ASTM D412
Tear Strength 22.8 kN/m
130 pli
ASTM D470
Graves Tear Strength 70.1 kN/m
400 pli
Die C; ASTM D624
Taber Abrasion, mg/1000 Cycles 22
22
H18, 1000g; ASTM D3389 B
Tensile Set 11 %
11 %
200% elongation; ASTM D412
Thermal Properties Metric English Comments
Melting Point 125 °C
257 °F
Kofler
130 °C
266 °F
DSC
Glass Transition Temp, Tg -50.0 °C
-58.0 °F
DSC
Optical Properties Metric English Comments
Haze 7.0 %
7.0 %
pressed between glass; ASTM D1003
Processing Properties Metric English Comments
Zone 1 166 °C
331 °F
Extrusion
Zone 2 171 °C
340 °F
Extrusion
Zone 3 177 °C
351 °F
Extrusion
Zone 4 182 °C
360 °F
Extrusion
Adapter Temperature 182 °C
360 °F
Extrusion
Die Temperature 182 °C
360 °F
Zone 1, Extrusion
182 °C
360 °F
Zone 2, Extrusion
Drying Temperature 104 °C
219 °F
Dry Time 2.00 - 4.00 hour
2.00 - 4.00 hour
Dew Point -40.0 °C
-40.0 °F
Descriptive Properties Value Comments
Volume Swell in Water 2%
24h/23°C, ASTM D471