Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength | 33.79 MPa | 4901 psi | ASTM D-412 |
Lubrizol Advanced Materials PEARLTHANE® 16N85UV Thermoplastic Polyurethane Elastomer
(discontinued **) PEARLTHANE® 16N85UV is a polyether-based TPU, containing an anti-UV additive, supplied in form of translucent, colorless, combining hardness with excellent mechanical properties and excellent hydro.. |