Mechanical Properties Metric English Comments
Tensile Strength 5.70 MPa
827 psi
ISO 37
Multibase TPSiV® 3111-60A Thermoplastic Elastomer
FEATURES & BENEFITS: Soft silky feel; Excellent abrasion and scratch resistance; Excellent bonding to PC, ABS; Hydrolysis resistant; FDA 21 CFR 177.2600 CompliantAPPLICATIONS: Solution for soft touc..
Tensile Strength 5.70 MPa
827 psi
DIN 53504-S1
P & P Technology CB 50 Carbon Loaded Silicone
Applications: Electrically conductive grades which when properly catalyzed can be considered for applications requiring conductivity such as EMI gaskets, conductive sheaths for ignition cable core,..
Tensile Strength 5.70 MPa
827 psi
Shin-Etsu Silicones LIMSâ„¢ KE2004-20A/B Elastomer
Information Provided by Shin-Etsu Silicones of America, Inc.
Tensile Strength 5.70 MPa
827 psi
20; ISO 37
BASF Elastollan 890 AN TPUR
Description: Thermoplastic Polyurethane Elastomers with excellent mechanical properties, outstanding wear resistance, high tear and tensile strength, good damping characteristics and a high resilien..
Tensile Strength 5.70 MPa
827 psi
ISO 37
AlphaGary Evoprene™ 081 Standard SBS Thermoplastic Elastomer Compound
The Evoprene™ Standard is a styrene-butadiene -styrene based thermoplastic elastomer.Applications: extruded door, window and furniture seals and rubbing strips, mats, bump stops, grommets, coat han..
Copyright © lookpolymers.com All Rights Reserved