Description: Thermoplastic Polyurethane Elastomers with excellent mechanical properties, outstanding wear resistance, high tear and tensile strength, good damping characteristics and a high resilience performance. Typical Applications: Polyester based for transparent films.Note: Quoted results are from measurements on injection molded test platens, post tempered for 20 hours at 100°CInformation provided by BASF
Physical Properties Metric English Comments
Density 1.22 g/cc
0.0441 lb/in³
ISO 1183-1-A
Mechanical Properties Metric English Comments
Hardness, Shore A 94
94
ISO 868
Tensile Strength 5.70 MPa
827 psi
20; ISO 37
10.0 MPa
1450 psi
100; ISO 37
22.5 MPa
3260 psi
300; ISO 37
50.0 MPa
7250 psi
ISO 37
Elongation at Break 550 %
550 %
ISO 37
Charpy Impact, Notched 20.0 J/cm²

@Temperature -30.0 °C
95.2 ft-lb/in²

@Temperature -22.0 °F
DIN ISO 179
NB

@Temperature 23.0 °C
NB

@Temperature 73.4 °F
DIN ISO 179
Tear Strength 120 kN/m
685 pli
DIN ISO 34-1/Bb
Abrasion 45
45
[mm<sup>3</sup>; ISO 4649
Compression Set 32 %

@Temperature 23.0 °C
32 %

@Temperature 73.4 °F
DIN EN ISO 815
43 %

@Temperature 70.0 °C
43 %

@Temperature 158 °F
DIN EN ISO 815
Optical Properties Metric English Comments
Transmission, Visible 90 %
90 %
transparent; thickness not quantified
Processing Properties Metric English Comments
Processing Temperature 175 - 220 °C
347 - 428 °F
Extrusion
Mold Temperature 20.0 - 70.0 °C
68.0 - 158 °F
Descriptive Properties Value Comments
Commercial Status North America
Primary Processing Technique Extrusion