Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength | 53.0 MPa | 7680 psi | ASTM D-638 |
Plaskolite Optix® CA - 41 HF General Purpose Acrylic Resin OPTIX® general purpose acrylics are available in a variety of performance grades that offer varying melt flow rates, heat resistance, color/opacity and gloss levels.Information provided by Plaskoli.. |
|||
Tensile Strength | 53.0 MPa | 7680 psi | ASTM D-638 |
Plaskolite Optix® CP - 41 HF General Purpose Acrylic Resin OPTIX® general purpose acrylics are available in a variety of performance grades that offer varying melt flow rates, heat resistance, color/opacity and gloss levels.Information provided by Plaskoli.. |
|||
Tensile Strength | 53.0 MPa | 7680 psi | ASTM D-638 |
Plaskolite West Optix® CP - 41 HF General Purpose Acrylic Resin Generally unaffected by alkalis, hydrocarbons, non-oxidizing acids, and salt water. Transparent, translucent, opaque, and custom colors in various grades of melt flow rate and heat resistance are av.. |
|||
Tensile Strength | 53.0 MPa | 7680 psi | ASTM D-638 |
Plaskolite West Optix® CA - 41 HF General Purpose Acrylic Resin Generally unaffected by alkalis, hydrocarbons, non-oxidizing acids, and salt water. Transparent, translucent, opaque, and custom colors in various grades of melt flow rate and heat resistance are av.. |
|||
Tensile Strength | 53.0 MPa @Temperature 23.0 °C |
7690 psi @Temperature 73.4 °F |
5mm/min (0.2in/min); ASTM D638 |
DuPont Performance Polymers Delrin® 100AF Acetal Homopolymer
(Unverified Data**) Delrin® 100AF is a high viscosity acetal homopolymer containing 20% Teflon® PTFE fibers. It is designed for applications requiring low wear and/or low friction against steel, itself, and other pla.. |
|||
Tensile Strength | 53.0 MPa | 7680 psi | ASTM D638 |
Gromax CCP PBT 1100-600S Product Description: PBT unreinforced high viscosity injection molding grade. Characteristics:Excellent electrical property Excellent temperature resistance, high heat distortion temperature. Excell.. |
|||
Tensile Strength | 53.0 MPa @Strain 5.00 %, Temperature 0.000 °C |
7690 psi @Strain 5.00 %, Temperature 32.0 °F |
50 mm/min; ISO 527-2 |
BASF Elastollan R 1000 20% Glass Filled TPUR Description: Thermoplastic Polyester Polyurethane Elastomers with exceptional properties, very high impact resistance, high modulus with at the same time elasticity, low coefficient of thermal expan.. |
|||
Tensile Strength | 53.0 MPa | 7690 psi | 5 mm/min; ISO 527-1 |
Sax Polymers SAXALEN PPC344G25 Polypropylene Copolymer, 25% Glass Filled SAXALEN PPC344G25 is a 25% glass filled Polypropylene - Copolymer intended for injection molding.Information provided by SAX Polymers |