Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Plaskolite Optix® CP - 41 HF General Purpose Acrylic Resin

Category Polymer , Thermoplastic , Acrylic (PMMA) , Acrylic, General Purpose, Molded , Acrylic, Optical Grade, Molded
Manufacturer Plaskolite
Trade Name Optix®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Plaskolite Optix® CP - 41 HF General Purpose Acrylic Resin.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
OPTIX® general purpose acrylics are available in a variety of performance grades that offer varying melt flow rates, heat resistance, color/opacity and gloss levels.Information provided by Plaskolite, Inc.
Physical Properties Metric English Comments
Density 1.19 g/cc
0.0430 lb/in³
ASTM D-792
Water Absorption 0.30 %
0.30 %
ASTM D-570
Linear Mold Shrinkage 0.0020 - 0.0060 cm/cm
0.0020 - 0.0060 in/in
ASTM D-955
Melt Flow 30 g/10 min

@Load 3.80 kg,
Temperature 230 °C
30 g/10 min

@Load 8.38 lb,
Temperature 446 °F
ASTM D-1238
Mechanical Properties Metric English Comments
Hardness, Rockwell M 74
74
ASTM D-785
Tensile Strength 53.0 MPa
7680 psi
ASTM D-638
Elongation at Break 2.4 %
2.4 %
ASTM D-638
Modulus of Elasticity 2.727 GPa
395.5 ksi
ASTM D-638
Flexural Strength 76.19 MPa
11050 psi
ASTM D-790
Izod Impact, Notched 0.160 J/cm

@Thickness 6.35 mm
0.300 ft-lb/in

@Thickness 0.250 in
ASTM D-256
Gardner Impact 0.226 J

@Thickness 3.17 mm
0.167 ft-lb

@Thickness 0.125 in
Falling Weight; ASTM D-3029 GB
Thermal Properties Metric English Comments
CTE, linear 60.0 µm/m-°C
33.3 µin/in-°F
ASTM D-696
Deflection Temperature at 1.8 MPa (264 psi) 71.7 °C
161 °F
ASTM D-648
Vicat Softening Point 88.9 °C
192 °F
ASTM D-1525
Flammability, UL94 HB
HB
Optical Properties Metric English Comments
Refractive Index 1.49
1.49
ASTM D-542
Haze <= 1.0 %
<= 1.0 %
ASTM D-1003
Transmission, Visible 92 %
92 %
ASTM D-1003
Users viewing this material also viewed the following: