Mechanical Properties Metric English Comments
Tensile Strength 0.400 MPa
58.0 psi
Shin-Etsu Silicones KE-1842 Silicone, RTV Adhesive/Sealant
Information Provided by Shin-Etsu Silicones of America, Inc.
Tensile Strength 0.400 MPa
58.0 psi
Shin-Etsu Silicones KE-200 Silicone, Potting/Encapsulation RTV
Information Provided by Shin-Etsu Silicones of America, Inc.
Tensile Strength 0.400 MPa
58.0 psi
ASTM D 412
Eurofoam Evacell XM 2001 EVA + PE Foam
Foamed polyethylene charged with EVA, with extremely fine cells, excellent elasticity, resilience and mechanical resistance. It can be thermoformed several times. It has completely closed cells, di..
Tensile Strength 0.400 MPa
58.0 psi
ASTM D 412
Eurofoam Gummicell GU 250 0,70 NR Foam
Natural rubber foam. Uses: industrial purposes, ceramics, mouse pads, diecutting, eletronics, and electromechanicsInformation provided by Eurofoam s.r.l.
Tensile Strength 0.400 MPa
58.0 psi
ASTM D 412
Eurofoam Porocell POR 304 F-7142 EPDM Foam
Ethylene Propylene Diene Monomer Foam. Used for thermal insulation and soundproofing, antivibration and waterproofing; different types of gaskets.Information provided by Eurofoam s.r.l.
Tensile Strength 0.400 MPa
58.0 psi
BASF Styrodur® 4000 CS Extruded Rigid Polystyrene Foam (Europe)
Description: Styrodur C is the green extruded rigid polystyrene foam (XPS) from BASF. As a thermal insulation, it makes a significant contribution to climate protection by reducing CO2 emissions. Th..