Tensile Strength 41.2 MPa
5970 psi
ASTM D638
GRECO ISOPAK 547M ABS Resin
Metal Plating GradeInformation provided by Greater Eastern Resins Industrial Co., Ltd.
Tensile Strength 41.2 MPa
5970 psi
50 mm/min; ISO 527-1,-2
Gromax BTE70-DN001N1 Nylon 6 (Dry)
Information provided by Gromax Enterprises Corp.