Material Notes:
Metal Plating GradeInformation provided by Greater Eastern Resins Industrial Co., Ltd.
Physical Properties Metric English Comments
Specific Gravity 1.03 g/cc
1.03 g/cc
ASTM D792
Water Absorption 0.30 %

@Temperature 23.0 °C,
Time 86400 sec
0.30 %

@Temperature 73.4 °F,
Time 24.0 hour
ASTM D570
Melt Flow 2.4 g/10 min

@Load 5.00 kg,
Temperature 200 °C
2.4 g/10 min

@Load 11.0 lb,
Temperature 392 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 105
105
ASTM D785
Tensile Strength 41.2 MPa
5970 psi
ASTM D638
Flexural Yield Strength 67.7 MPa
9810 psi
ASTM D790
Flexural Modulus 2.45 GPa
356 ksi
ASTM D790
Izod Impact, Notched 2.35 J/cm
4.41 ft-lb/in
ASTM D256 A
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 85.0 °C
185 °F
ASTM D648
Flammability, UL94 HB
HB