Mechanical Properties Metric English Comments
Tensile Strength 60.01 MPa
8703 psi
Bulk Molding Compounds BMC T40(25)-XHS-15869 Die Casting Replacement Grade Molding Compound
BMC T40(25)-XHS-15869 is a high strength molding compound with excellent dimensional stability. It is UL recognized and is available in a wide range of colors. Because of its superior physical pro..