Category Polymer , Thermoset , Polyester, TS , Polyester (Thermoset) - Rigid
Manufacturer BMC - Bulk Molding Compounds Inc.
Trade Name BMC
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Bulk Molding Compounds BMC T40(25)-XHS-15869 Die Casting Replacement Grade Molding Compound.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
BMC T40(25)-XHS-15869 is a high strength molding compound with excellent dimensional stability. It is UL recognized and is available in a wide range of colors. Because of its superior physical properties and ability to maintain machined tolerances in a molding part it is used widely as a direct replacement for die castings. T40(25)-XHS-15869 can be injection, compression and transfer molded. Other uses are structural parts as well as circuit breakers.Information provided by Bulk Molding Compounds, Inc.
Physical Properties Metric English Comments
Density 1.71 - 1.78 g/cc
0.0618 - 0.0643 lb/in³
Molded
Linear Mold Shrinkage 0.00050 - 0.0015 cm/cm
0.00050 - 0.0015 in/in
Mechanical Properties Metric English Comments
Hardness, Barcol 40 - 50
40 - 50
Tensile Strength 60.01 MPa
8703 psi
Flexural Strength 111.32 MPa
16146 psi
Flexural Modulus 10.3 GPa
1500 ksi
Compressive Strength 131 MPa
19000 psi
Izod Impact, Notched 5.160 J/cm
9.664 ft-lb/in
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) >= 260 °C
>= 500 °F
Flammability, UL94 V-0
V-0
UL 94 V0/UL 94 5V
Electrical Properties Metric English Comments
Dielectric Strength 13.2 - 15.2 kV/mm
335 - 385 kV/in
short time
Arc Resistance >= 183 sec
>= 183 sec
Comparative Tracking Index >= 500 V
>= 500 V
Processing Properties Metric English Comments
Processing Temperature 138 - 166 °C
280 - 330 °F