Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength 621 - 758 MPa

@Thickness >=25.4 mm
90000 - 110000 psi

@Thickness >=1.00 in
Turned Bars
Schmolz + Bickenbach 416 Stainless Steel Bar
Description: Ugitech’s 416 is free machining martensitic grade. The unique production process—developed exclusively by Ugitech—results in a product that delivers superior productivity..
Tensile Strength 621 - 827 MPa

@Thickness <=25.4 mm
90000 - 120000 psi

@Thickness <=1.00 in
Cold Drawn Bars
Schmolz + Bickenbach 416 Stainless Steel Bar
Description: Ugitech’s 416 is free machining martensitic grade. The unique production process—developed exclusively by Ugitech—results in a product that delivers superior productivity..
Tensile Strength >= 621 MPa
>= 90000 psi
Eagle Brass 200/201 Nickel Alloy, Full Hardened
Nickel 200/201 has properties that are useful in industries such as chemical processing and electronics. Nickel is resistant to various reducing chemicals and alkaline materials. Compared with nick..
Tensile Strength 621 - 689 MPa
90000 - 100000 psi
Eagle Brass 430 Ferritic Stainless Steel, 1/2 Hardened
Type 430 is one of the most widely used of the "non-hardenable" ferritic stainless steels. It combines good corrosion resistance and heat and oxidation with good mechanical properties. Typical pro..
Tensile Strength 621 - 724 MPa
90000 - 105000 psi
Chicago Extruded Metals BioBrass® UNS C62400 Aluminum Bronze
Finished product available as rod or forged.Chicago Extruded Metal temper codes: H02, M30This alloy is registered with the U.S. EPA as Antimicrobial.Information provided by Chicago Extruded Metals
Tensile Strength 621 - 814 MPa
90000 - 118000 psi
Chicago Extruded Metals BioBrass® UNS C63000 Aluminum Bronze
Finished product available as bar,rod, forged, shapes, or tubes.Chicago Extruded Metal temper codes: H02, M30This alloy is registered with the U.S. EPA as Antimicrobial.Information provided by Chica..