Material Notes:
Finished product available as rod or forged.Chicago Extruded Metal temper codes: H02, M30This alloy is registered with the U.S. EPA as Antimicrobial.Information provided by Chicago Extruded Metals
Physical Properties Metric English Comments
Density 7.45 g/cc
0.269 lb/in³
Mechanical Properties Metric English Comments
Hardness, Rockwell B 87 - 92
87 - 92
Tensile Strength 621 - 724 MPa
90000 - 105000 psi
Tensile Strength, Yield 276 - 359 MPa
40000 - 52000 psi
Elongation at Break 14 - 18 %
14 - 18 %
Thermal Properties Metric English Comments
Thermal Conductivity 86.5 W/m-K
600 BTU-in/hr-ft²-°F
Component Elements Properties Metric English Comments
Aluminum, Al 10 - 11.5 %
10 - 11.5 %
Copper, Cu >= 82.75 %
>= 82.75 %
as balance
Iron, Fe 2.0 - 4.5 %
2.0 - 4.5 %
Manganese, Mn <= 0.30 %
<= 0.30 %
Other, total 0.50 %
0.50 %
Silicon, Si <= 0.25 %
<= 0.25 %
Tin, Sn <= 0.20 %
<= 0.20 %
Electrical Properties Metric English Comments
Electrical Resistivity 0.0000144 ohm-cm
0.0000144 ohm-cm