Mechanical Properties Metric English Comments
Tensile Strength 4.30 MPa
624 psi
Shin-Etsu Silicones KE-1830 Silicone, RTV Adhesive/Sealant
Information Provided by Shin-Etsu Silicones of America, Inc.
Tensile Strength 4.30 MPa
624 psi
ASTM D 638
API Megol AM DP2433/50PBT SEBS Adhesion Modified Overmolding for Polyesters
Over-molding allows for the creation of composite finished products in a single phase, removing the need for successive gluing or mechanical fixing steps. This also reduces environmental impact as ..