Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength | 64.7 MPa | 9390 psi | ASTM D638 |
Samyang Tramid® 910 PA66/PA6 Strong with excellent thermal resistance. Abrasion resistance, chemical resistance and oil resistance are excellent.Applications:Automotive knob types, door handles and mirror housingsConnectorsCab.. |
|||
Tensile Strength | 64.7 MPa | 9390 psi | ASTM D638 |
Samyang Trirex® 3020A Polycarbonate with Heat Stabilizer PC is characterized by its excellent impact resistance, dimensional stability and excellent thermal resistance.3020A is a high flow grade with heat stabilizers.Information provided by Samyang. |
|||
Tensile Strength | 64.7 MPa | 9390 psi | ASTM D638 |
Samyang Trirex® 3020IR Polycarbonate with Heat Stabilizer PC is characterized by its excellent impact resistance, dimensional stability and excellent thermal resistance.3020IR is a high flow grade with added heat stabilizers, separating materials and stain.. |
|||
Tensile Strength | 64.7 MPa | 9390 psi | ASTM D638 |
Samyang Trirex® 3020PJ Polycarbonate PC is characterized by its excellent impact resistance, dimensional stability and excellent thermal resistance.3020PJ is a high flow grade.Information provided by Samyang. |
|||
Tensile Strength | 64.7 MPa | 9390 psi | ASTM D638 |
Samyang Trirex® 3020U UV Stable Polycarbonate PC is characterized by its excellent impact resistance, dimensional stability and excellent thermal resistance.3020U is a high flow, UV Stable grade.Information provided by Samyang. |
|||
Tensile Strength | 64.7 MPa | 9390 psi | ASTM D638 |
Samyang Trirex® 3020R Polycarbonate with Heat Stabilizer PC is characterized by its excellent impact resistance, dimensional stability and excellent thermal resistance.3020R is a high flow grade with added heat stabilizers and separating materials.Informa.. |