Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength | 68.67 MPa | 9960 psi | ASTM D638 |
E-Polymers TEKAFIN® PH70G1 HIPP + 10% Glass Fiber Reinforced Scratch Resistance Compounded-PP Modified PP: TEKAFIN is modified PP resins formulated with various fillers and modifiers. It has product lines for impact modified, glass fiber reinforced, inorganic filler reinforced and hybrids.I.. |
|||
Tensile Strength | 68.67 MPa | 9960 psi | ASTM D638 |
E-Polymers TEKALOY® S630XB Heat Resistance, Weatherability PC/PBT Alloy PC/ABS, PC/PBT, PC/PET: TEKALOY is high performance polymer alloy resins (PC/ABS, PC/PBT, and PC/PET, etc) manufactured by E-Polymers. PC/ABS has excellent mechanical properties, high heat resistan.. |
|||
Tensile Strength | 68.67 MPa | 9960 psi | ASTM D638 |
E-Polymers SEPAZ® N3040HI Nanoclay 4% High Impact Nano Composite Resin Nanocomposite: SEPAZ Nano PA6 nanocomposites have been prepared successfully in commercial scale through 'in situ' polymerization or melt extrusion. The unique performance properties of nanocomposi.. |