Polymer Property : Tensile Strength = 696 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength >= 4.80 MPa
>= 696 psi
in the plane; ISO 527 1-2
3A Composites Core Materials AIREX® C70.200 Universal Structural Foam
AIREX® C70 is a closed cell, crosslinked polymer foam that combines excellent stiffness and strength to weight ratios with superior toughness. It is non-friable, contains no CFC’s, has negli..
Tensile Strength 4.80 MPa
696 psi
20; ISO 37
BASF Elastollan 1085 A TPUR
Description: Thermoplastic Polyurethane Elastomers with excellent mechanical properties, outstanding wear resistance, high tear and tensile strength, good damping characteristics and a high resilien..
Tensile Strength 4.80 MPa
696 psi
ASTM D 638
API Megol AM DP2392/40 SEBS Adhesion Modified Overmolding for Polar Polymers
Over-molding allows for the creation of composite finished products in a single phase, removing the need for successive gluing or mechanical fixing steps. This also reduces environmental impact as ..
Tensile Strength 4.80 MPa
696 psi
ISO 37
AlphaGary Evoprene™ CE 6186 Thermoplastic Elastomer
The Evoprene™ CE range has been specially created to offer processors a cost engineered range of easy processing, fast cycling thermoplastic elastomer compounds for general purpose applications. E..
Tensile Strength 4.80 MPa
696 psi
ISO 37
AlphaGary Evoprene™ 075 Standard SBS Thermoplastic Elastomer Compound
The Evoprene™ Standard is a styrene-butadiene -styrene based thermoplastic elastomer.Applications: extruded door, window and furniture seals and rubbing strips, mats, bump stops, grommets, coat han..
Tensile Strength 4.80 MPa
696 psi
ISO 37
AlphaGary Evoprene™ 076 Standard SBS Thermoplastic Elastomer Compound
The Evoprene™ Standard is a styrene-butadiene -styrene based thermoplastic elastomer.Applications: extruded door, window and furniture seals and rubbing strips, mats, bump stops, grommets, coat han..
Tensile Strength 4.80 MPa
696 psi
ISO 37
AlphaGary Evoprene™ GC 5683 SEBS Thermoplastic Elastomer
Evoprene™ GC compounds are based on styrene ethylene- butylene styrene block copolymers. Evoprene™ GC series was created to provide cost effective solutions for processors and end users alike. Can..