Material Notes:
The Evoprene™ Standard is a styrene-butadiene -styrene based thermoplastic elastomer.Applications: extruded door, window and furniture seals and rubbing strips, mats, bump stops, grommets, coat hanger pads, toy components
Physical Properties Metric English Comments
Specific Gravity 1.10 g/cc
1.10 g/cc
ISO 2782
Viscosity Measurement 20

@Temperature 150 °C
20

@Temperature 302 °F
Kg/cm<sup>2</sup>; Macklow-Smith extrusion rheometer
Mechanical Properties Metric English Comments
Hardness, Shore A 60
60
ISO 868
Tensile Strength 4.80 MPa
696 psi
ISO 37
Elongation at Break 610 %
610 %
ISO 37
100% Modulus 0.00170 GPa
0.247 ksi
ISO 37
Tear Strength 27.0 kN/m
154 pli
ISO 34-B
Compression Set 18 %

@Temperature 22.0 °C,
Time 259000 sec
18 %

@Temperature 71.6 °F,
Time 72.0 hour
ISO 815
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 55.0 - 60.0 °C
131 - 140 °F
Minimum Service Temperature, Air -60.0 °C
-76.0 °F
Descriptive Properties Value Comments
Bonds with Polystyrene
Chemical Resistance Acetone
Moderate
Acids up to 80%
Moderate
Alcohol
Good
Alkalis
Good
Brake fluid
Moderate
Chlorinate solvents
Poor
Diesel
Poor
Ethylene glycol
Excellent
Gasoline
Poor
Salt solution
Good
Soda lye
Moderate
Water, 23°C
Good
Water, 95°C
Poor
Ozone Resistance Pass - No Crack
100 pphm / 200 hrs / 20% strain
Transparency Opaque