Material Notes:
Waterborne, corrosion-inhibiting primer, maintains surface bondability after multiple prebonding cure cycles. Meets SCAQMD Rule 1124. Replacement for Hysol EA 9210B.Applications: Sprayable Low Viscosity Wet Lay-up Metal and Honeycomb Bonding
Physical Properties Metric English Comments
Storage Temperature 5.00 °C
41.0 °F
Mechanical Properties Metric English Comments
Tensile Strength 8.00 MPa
1160 psi
Flatwise
Adhesive Bond Strength 13.8 MPa

@Temperature 177 °C
2000 psi

@Temperature 351 °F
Lap Shear
33.1 MPa

@Temperature -55.0 °C
4800 psi

@Temperature -67.0 °F
Lap Shear
34.5 MPa

@Temperature 25.0 °C
5000 psi

@Temperature 77.0 °F
Lap Shear
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 177 °C
351 °F
Processing Properties Metric English Comments
Cure Time 60.0 min

@Temperature 132 °C
1.00 hour

@Temperature 270 °F
Descriptive Properties Value Comments
Honeycomb Climbing Drum Peel, mN/m 60
at 25°C
Out-Time (days) 30
at 25°C
Primer Coverage, sq.m/L 416
at 8µm dry film thickness