Tensile Strength 8.62 MPa
1250 psi
ASTM D638
S&E Specialty Polymers G-94-142A PVC
Application: Flexible Clear PVC based compound for extrusion and molding application.Information provided by S&E Specialty Polymers
Tensile Strength 8.62 MPa
1250 psi
ASTM D412
S&E Specialty Polymers TufGuard E™ XP-115DD-Zeta PE, Flame Retardant
Application: Chlorinated PE TPO based compound suitable for Wire and Cable applications.Information provided by S&E Specialty Polymers
Tensile Strength 8.62 MPa
1250 psi
ASTM D412
S&E Specialty Polymers TufGuard E™ XP-115D-Zeta PE, Flame Retardant
Application: Chlorinated PE TPO based compound suitable for Wire and Cable applications.Information provided by S&E Specialty Polymers
Tensile Strength 8.62 MPa
1250 psi
ASTM D412
Northstar Polymers MPP-D65A Polyether Base Polyurethane Resin
MPP-D65A is a polyether base 2-component polyurethane resin casting system for molding and potting applications. It has a long pot-life and gradual curing pattern to provide easier handling for mol..
Tensile Strength 8.62 MPa

@Strain 100 %
1250 psi

@Strain 100 %
510 mm/min; ASTM D638
PolyOne Geon™ Vinyl Flexible B8502 Polyvinyl Chloride, Flexible (PVC, Flexible)
A flexible PVC Compound with good resistance to migration to specific applications.Information provided by PolyOne
Tensile Strength 8.62 MPa
1250 psi
Teknor Apex Elexar® EL 3954-90 Thermoplastic Elastomer
Notes: Elexar® is a family of styrene block copolymer thermoplastic elastomers, often referred to as thermoplastic rubber (TPR). Elexar® "rubber-like" compounds offer superior electrical prop..
Tensile Strength 8.62 MPa
1250 psi
Compound Property; ASTM D412
Arlon 10842S018 0.018" (0.457 mm) Fully Cured, Unsupported, Silicone Rubber
Design/Construction:Side 1: Fully Cured, Unsupported, Silicone Rubber Appearance: Dark red silicone rubberThis data represents typical values for the production material. The data should not be used..
Tensile Strength 8.62 MPa
1250 psi
Silicone Property; Arlon SQA-TMS-008
Arlon 55833R062 Mar Resistant Press Pad; 1.6 mm Cured Silicone Rubber with Fiberglass Substrate
Mar Resistant Press Pad - Product is sold with two finishes options: 55833R062AC - "C-finish" and 55833R062DST - "Smooth with Talc"Design/Construction:Interleave: 3 mil PESide 1: Cured Silicone Ru..
Tensile Strength 8.62 MPa
1250 psi
Silicone Property; ASTM D412
Arlon R37292S018 0.018" (0.457 mm) Cured Silicone Rubber with PTFE Coated Fiberglass Substrate