Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength | 8.96 MPa @Strain 100 % |
1300 psi @Strain 100 % |
Type IV, 510 mm/min; ASTM D638 |
PolyOne Geon™ Vinyl Wire & Cable JAL110A Natural Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Tensile Strength | 8.96 MPa | 1300 psi | ASTM D638 |
Quadrant EPP Fluorosint® 135 PTFE and PPS Blend, with Proprietary Lubrication Fillers (ASTM Product Data Sheet) Chemical resistance parallels PTFE Continuous use temperatures to 500°F (260°C) Compared to PTFE higher load carrying capability 1/9 of the deformation under load lower coefficient of thermal exp.. |
|||
Tensile Strength | 8.96 MPa @Strain 100 % |
1300 psi @Strain 100 % |
Type IV, 510 mm/min; ASTM D638 |
PolyOne Geon™ Vinyl Flexible A8001 Polyvinyl Chloride, Flexible (PVC, Flexible) Recommended for interior applications.Information provided by PolyOne |
|||
Tensile Strength | 8.96 MPa @Strain 100 % |
1300 psi @Strain 100 % |
510 mm/min; ASTM D638 |
PolyOne Geon™ Vinyl Flexible B8503 Polyvinyl Chloride, Flexible (PVC, Flexible) A flexible PVC Compound with good resistance to migration to specific applications.Information provided by PolyOne |
|||
Tensile Strength | 8.96 MPa @Strain 100 % |
1300 psi @Strain 100 % |
510 mm/min; ASTM D638 |
PolyOne Geon™ Vinyl Flexible C9000 Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Tensile Strength | 8.96 MPa @Strain 100 % |
1300 psi @Strain 100 % |
510 mm/min; ASTM D638 |
PolyOne Geon™ Vinyl Flexible C90A0 Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Tensile Strength | 8.96 MPa @Strain 100 % |
1300 psi @Strain 100 % |
510 mm/min; ASTM D638 |
PolyOne Geon™ Vinyl Flexible C90B1 Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Tensile Strength | 8.96 MPa @Strain 100 % |
1300 psi @Strain 100 % |
Type IV, 510 mm/min; ASTM D638 |
PolyOne Geon™ Vinyl Flexible C90UB Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Tensile Strength | 8.96 MPa | 1300 psi | Typical |
Garlock 2102 C.I. SBR/NBR Sheet Rubber, Polyester Insert Garlock cloth-inserted materials are designed to add stability where mechanical fastening is necessary, and to reduce gasket creep where heavy flange loading is required.Style #2102 C.I. is a smooth.. |
|||
Tensile Strength | 8.96 MPa | 1300 psi | Typical |
Garlock 2103 C.I. SBR/NBR Sheet Rubber, Polyester Insert Garlock cloth-inserted materials are designed to add stability where mechanical fastening is necessary, and to reduce gasket creep where heavy flange loading is required.Style #2103 C.I. is a smooth.. |
|||
Tensile Strength | 8.96 MPa | 1300 psi | Typical |
Garlock Viton® 501 Fluoroelastomer Sheet Rubber Style #501 sheet rubber, made with VITON® fluoroelastomer, is a high-performance product resistant to heat, oils, fuels, numerous acids and other chemicals.Information provided by Garlock Rubber .. |
|||
Tensile Strength | 8.96 MPa | 1300 psi | ASTM D638 |
Ineos A60-70-162 HDPE Ineos A60-70-162 is a high density polyethylene homopolymer, developed specifically for blow molding food containers on reciprocating screw-type equipment. It exhibits excellent processing character.. |
|||
Tensile Strength | 8.96 MPa | 1300 psi | Typical values on polymer compression molded at 350ºF; ASTM D412 |
Kraton® D4158 K (O/E SBS) Radial Copolymer Description: Kraton D4158 K is an oiled, radial copolymer based on styrene and butadiene with a polystyrene content of 31%. It is supplied from North America in the physical form: Kraton D4158 KT - .. |
|||
Tensile Strength | 8.96 MPa | 1300 psi | |
Teknor Apex Elexar® EL 1934D Thermoplastic Elastomer Notes: Elexar® is a family of styrene block copolymer thermoplastic elastomers, often referred to as thermoplastic rubber (TPR). Elexar® "rubber-like" compounds offer superior electrical prop.. |
|||
Tensile Strength | 8.96 MPa | 1300 psi | |
Teknor Apex Elexar® EL 1934C Thermoplastic Elastomer Notes: Elexar® is a family of styrene block copolymer thermoplastic elastomers, often referred to as thermoplastic rubber (TPR). Elexar® "rubber-like" compounds offer superior electrical prop.. |
|||
Tensile Strength | 8.96 MPa | 1300 psi | |
Teknor Apex Elexar® EL 1934F Thermoplastic Elastomer Notes: Elexar® is a family of styrene block copolymer thermoplastic elastomers, often referred to as thermoplastic rubber (TPR). Elexar® "rubber-like" compounds offer superior electrical prop.. |
|||
Tensile Strength | 8.96 MPa | 1300 psi | |
Teknor Apex Elexar® EL 1934G Thermoplastic Elastomer Notes: Elexar® is a family of styrene block copolymer thermoplastic elastomers, often referred to as thermoplastic rubber (TPR). Elexar® "rubber-like" compounds offer superior electrical prop.. |
|||
Tensile Strength | 8.96 MPa | 1300 psi | |
Teknor Apex Tekbond® TB 2005 Thermoplastic Elastomer Notes: Tekbond® TPEs are a functional series of elastomer compounds designed to not only bond to the most difficult neat and reinforced engineering substrates with no primer or surface treatment, b.. |
|||
Tensile Strength | 8.96 MPa | 1300 psi | Silicone; ASTM D412 |
Arlon 25662T010 0.010" (0.254 mm) Cured Silicone Rubber with Laminated ETFE Film Substrate Design/Construction:Side 1: Cured Silicone RubberSubstrate: Laminated ETFE FilmChemical Compatibility: (ETFE offers good chemical resistance to the following classes of chemicals) Alkalis, Organic a.. |
|||
Tensile Strength | 8.96 MPa | 1300 psi | Silicone Property; ASTM D412 |
Arlon 30400N060 0.060" (1.52 mm) Uncured Silicone Rubber Design/Construction: Interleave 1: KodacelProduct: Uncured Silicone Rubber Interleave 2: Polyethylene Appearance: Translucent silicone rubber on polymer linerThis data represents typical values for .. |
|||
Tensile Strength | 8.96 MPa | 1300 psi | Silicone Property; ASTM D412 |
Arlon 99790N010 0.010" (0.254 mm) Uncured Silicone Rubber with PTFE Coated Fiberglass Carrier Design/Construction: Liner: FEP Side 1: Uncured Silicone Rubber Carrier: PTFE Coated FiberglassThis data represents typical values for the production material. The data should not be used to write,.. |
|||
Tensile Strength | 8.96 MPa | 1300 psi | |
AlphaGary Garaflex™ O 9949 RA Olefinic Thermoplastic Elastomer Garaflex™ O is a flame retarded, olefinic thermoplastic elastomer105°C rated flame retardant olefinic TPE for flat ribbon cable and heat tracing cable |
|||
Tensile Strength | 8.96 MPa | 1300 psi | |
AlphaGary Garathane™ GT 5080 A Polyurethane based compound PVC/PU Alloy dull finish |
|||
Tensile Strength | 8.96 MPa | 1300 psi | Compound Property |
Arlon R34020W062 0.062" (1.57 mm) Uncured, Unsupported Silicone Rubber on a Kodacel Carrier Design/Construction:Side 1: Uncured, Unsupported Silicone Rubber on a Kodacel Carrier This data Represents typical values for the production material. The data should not be used to write, or in pla.. |
|||
Tensile Strength | 8.96 MPa | 1300 psi | Silicone Property; ASTM D412 |
Arlon 32400N030 0.030" (0.762 mm) Uncured Silicone Rubber on PET Carrier Design/Construction: Interleave: PolyethyleneSide 1: Uncured Silicone RubberCarrier: PET Appearance: Translucent silicone rubber on polymer linerThis data represents typical values for the productio.. |
|||
Tensile Strength | 8.96 MPa | 1300 psi | Silicone Property; ASTM D412 |
Arlon 32400N060 0.060" (1.52 mm) Uncured Silicone Rubber Design/Construction: Interleave 1: PET carrierSide 1: Uncured Silicone RubberInterleave 2 : PE carrierAppearance: Translucent silicone rubber on polymer linerThis data represents typical values for .. |
|||
Tensile Strength | 8.96 MPa | 1300 psi | Silicone Property; ASTM D412 |
Arlon R36613N022 0.022" (0.559 mm) Cured Silicone Rubber with Fiberglass Substrate Design/Construction: Side 1: Cured Silicone Rubber Substrate: Style 7628 Heat Cleaned FiberglassSide 2: Cured Silicone RubberSide 2 Interleave: PolyethyleneFiberglas Weave: PlainThis data represents.. |
|||
Tensile Strength | 8.96 MPa | 1300 psi | Silicone Property; ASTM D412 |
Arlon R36812T010 0.010" Cured Silicone Rubber with Laminated ETFE Film Substrate Design/Construction:Liner: N/ASide 1: Cured Silicone RubberSubstrate: Laminated ETFE FilmChemical Compatibility: Alkalis, Organic and Inorganic acids, Amines, Epoxies, Aromatic compounds, Chlorin.. |
|||
Tensile Strength | 8.96 MPa | 1300 psi | Silicone Property; ASTM D412 |
Arlon R37223N008 0.008" (0.203 mm) Cured Silicone Rubber with Fiberglass Substrate Design/Construction: Side 1: Cured Silicone Rubber Substrate: Style 1653 Heat Cleaned Fiberglass ScrimSide 2: Cured Silicone RubberFiberglass Scrim Weave: LenoThis data represents typical values for.. |