Polymer Property : Tensile Strength = 83.4 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength 83.4 MPa
12100 psi
ASTM D638
Solvay Specialty Polymers Amodel® AT-1002 HS Polyphthalamide (PPA)  (Unverified Data**)
Amodel AT-1002 HS is a neat, toughened, heat stabilized polyphthalamide (PPA) resin that offers superior retention of properties after humid thermal aging; high impact at low temperature and better ..
Tensile Strength 83.4 MPa
12100 psi
ASTM D638
Gromax CCP ABS/PBT 7320H-104 20% Glass Fiber Filled
Product Description: A 20% glass fiber reinforced injection molding grade. Characteristics:Low warp age and excellent dimensionally stable Excellent electrical property Excellent mechanic and chemi..
Tensile Strength 83.4 MPa
12100 psi
ASTM D638
Solvay Specialty Polymers Amodel® AT-1002 HS Polyphthalamide (PPA)
Amodel® AT-1002 HS is a neat, toughened, heat stabilized polyphthalamide (PPA) resin that offers superior retention of properties after humid thermal aging; high impact at low temperature and bet..
Tensile Strength 83.4 MPa
12100 psi
ASTM D638
Samyang Tribit® 1500G15K PBT, Reinforced Impact
Crystallization is fast, formability is excellent and thermal resistance, chemical resistance, electrical properties and abrasion resistance are excellent.1500G15K is a reinforced, impact grade.Appl..
Tensile Strength 83.4 MPa
12100 psi
ASTM D638
Shinkong Synthetic Fibers Shinite® P305G30 PP, 30% Glass Filled
Information from Shinkong Synthetic Fibers Corp.
Tensile Strength 83.4 MPa
12100 psi
ASTM D638
Shinkong Synthetic Fibers Shinite® P305G30 PP, 30% Glass Filled
Information from Shinkong Synthetic Fibers Corp.
Tensile Strength 83.4 MPa
12100 psi
ASTM D638
Samyang Triloy® S460G15 Polymer Alloy, Reinforced
Excellent impact, formability and weather resistance.220 is a reinforced grade.Applications: LCD Panel Frame - for dimensional stabilityInformation provided by Samyang.