Mechanical Properties Metric English Comments
Compressive Strength 0.300 - 0.400 MPa
43.5 - 58.0 psi
Green strength
ICHS Fiberfax® Alumina-Silica Ceramic Fibers
Fiberfrax® ceramic fibers are made from high-purity alumina-silica materials. ICHS uses Fiberfrax® ceramic fiber to manufacture vacuum-formed products in:High-Temperature DuctworkCombustion C..
Compressive Strength 0.300 MPa
43.5 psi
Dried at 110°C (230°F)
Skamol Group VERMICAST 116-25 Insulating Castable
SKAMOL insulating castables have the following characteristics: Max. service temperature: Up to 1100°C (2102°F)Back-up insulation or hot-face usesFor casting and gunningProducts are based on f..
Compressive Strength 0.300 MPa
43.5 psi
Lower Yield in the Through Plane Direction
Cymat A35620SC 020SS Stabilized Aluminum Foam
Description: Cymat A35620SC 020SS stabilized aluminum foam (SAF) is a closed cell aluminum foam formed from A356 aluminum alloy with a density of 0.2 g/cm3. The mechanical properties of SAF make it ..
Compressive Strength 0.300 - 7.00 MPa
43.5 - 1020 psi
Dependent on grade
Destech Open-Celled Glassy Carbon Foam
Destech glassy (vitreous) carbon foam is available in different grades depending on the number of pores per inch (ppi). Standard grades are 10, 45, 100 and 500 ppi. Custom grades are available on a..
Compressive Strength 0.300 MPa

@Strain 10.0 %
43.5 psi

@Strain 10.0 %
DIN EN 826
BASF Styrodur® 3035 CS Extruded Rigid Polystyrene Foam (Europe)
Description: Styrodur C is the green extruded rigid polystyrene foam (XPS) from BASF. As a thermal insulation, it makes a significant contribution to climate protection by reducing CO2 emissions. Th..