Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Strength | 0.317 MPa | 46.0 psi | at 25%, Extruded; ASTM D3575, Suffix D |
Dow STRANDFOAM™ EA 1000 Polypropylene Foam STRANDFOAM™ EA 1000 Energy Absorbing polypropylene foam is a strong, low-density, closed-cell foam. It is suited as a component material in products requiring a shock and energy absorbing or vibra.. |