Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Strength | 1.90 MPa | 276 psi | Cold Crush Strength; ASTM C133 |
BNZ Materials BNZ-26 Insulating Firebrick BNZ produces many types of Insulating Fire Brick (IFB) for use in applications from 2,000°F (1,093°C) to 3,200°F (1,760°C). Each type is formulated to meet specific thermal and physical requirem.. |
|||
Compressive Strength | 1.90 MPa | 275 psi | |