Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Strength | 1.90 MPa | 275 psi | |
BNZ Materials 2645LI Insulating Aggregate BNZ manufactures a variety of insulating and dense castable refractories to meet the exacting needs of the high temperature processing industries. These hydraulic setting products are suitable for i.. |